RESEARCH OF PHASE-TRANSITIVE MATERIALS BY THE EXPERIMENTAL METHODS
Description
The article is devoted to the application of method of differential-scanning microcalorimetry for research of phase-transitive materials on the base of inorganic and organic substances.